C-CUTTER MINI Cutting Conditions
Feed (IPT)
Cutting Speed (SFM)
Material
Insert Grade
Coolant
Chamfering Face Milling
Stainless Steel, Carbon Steel, Alloy Steel
ACP200, ACP300
330-1150 330-655 265-525 165-260 330-825 130-195 65-100 330-1155 330-2640
.002-.016 .002-.016 .002-.016 .002-.016 .003-.012 .001-.003 .001-.003 .004-.020 .004-.020
.002-.008 .002-.008 .002-.008 .002-.008 .003-.008 .001-.003 .001-.003 .002-.010 .002-.012
Dry Dry Dry Dry
Alloy Tool Steel
Pre-hardened Steel, Hardened steel <HRC50
CWS20A
Hardened Steel HRC50-62
Stainless Steel
Dry/Wet
Titanium
ACM250F
Wet Wet Dry
Inconel
Cast Iron
NF15KA
Aluminum/Non-Ferrous
DS20, ACP300
Dry/Wet
• This table is a guideline for selecting cutting parameters; adjust them as needed according to the machine and workpiece conditions. • Generally, wet cutting effectively improves finishing surfaces • Wet cutting effectively suppresses built-up edges occurring on stainless steel or aluminum chamfering • For aluminum/non-ferrous materials marked with DS20 is the No.1 recommendation; if chatter occurs with DS20, use ACP300
For Spot Facing Hole Type And Long Type Of Bolt Hole & Tap Starting Hole Type
Cutting Speed (SFM)
Material
Insert Grade
Feed (IPT)
Coolant
Unalloyed Steel, Carbon Steel, Alloy Steel
ACP200 ACP300
66-330 165-525 99-330
.001-.005 .002-.008 .001-.005
Wet Dry Wet
Cast Iron
NF15KA
Aluminum/Non-ferrous
ACP200, ACP300
• This table is a guideline for selecting cutting parameters. Adjust them as needed according to the machine and workpiece conditions • Short projection length types other than the LONG TYPE are recommended for stainless steel and pre-hardened steel
539